Austenitic stainless steel refers to stainless steel with an austenitic structure at room temperature. When the steel contains about 18% Cr, 8%-25% Ni, and about 0.1% C, it has a stable austenite structure. Austenitic stainless steel is non-magnetic and has high toughness and plasticity, but its strength is low. It is impossible to strengthen it through phase transformation. It can only be strengthened by cold working. If elements such as S, Ca, Se, Te are added, it has good Machinability.
Specification
Classification | Hot Rolled Stainless Steel; Cold Rolled Stainless Steel |
Steel Grade | SUS304; SUS304L; SUS316L; SUS321 |
Thickness(mm) | 3.0-8.0 |
Width(mm) | 900-3200 |
Standard | JIS4304-2005; JIS4305-2005; EN10088-2; ASTM A240/240M; GB/T4237-2007; GB/T3280-2007; GB24511-2009; ASTM A480/480M |
Surface Treatment | NO.1; 2E; 2B; 2D; NO.3; NO.4; HL; HT |